On the above site you can download (after paying!) some good procedures such as:
 
1. WPS-FC-1 All position Flux-core on A36 plate using E71T-1 and 75-25 Ar/Co2.
2. WPS-FC-2 All position Flux-core on A36 plate using E71T-1 and 100% Co2.
3. WPS-FC-3 All position Flux-core on A240(316L) plate using E316LT-1 and 75-25 Ar/Co2.
4. WPS-FC-5 All position Flux-core on A240 (304L) plate using E308LT-1 and 75-25 Ar/Co2.
5. WPS-FC-6 All position Flux-core on A36 plate using E71T-8 without gas coverage.
6. WPS-GTAW-2 All position Tig on A240(304L) plate using ER308L with 100% Argon.
7. WPS-GTAW-2F All position dual process (Tig root/flux-core fill) on A240(304L) plate.
8. WPS-GTAW-2S All position dual process (Tig root/stick fill) on A240(304L) plate.
9. WPS-GTAW-3 All position Tig on A240(316L) plate using ER316L with 100% Argon.
10. WPS-GTAW-3F All position dual process (Tig root/flux-core fill) on A240(316L) plate.
11. WPS-GTAW-3S All position dual process (Tig root/stick fill) on A240(316L) plate.
12. WPS-SAW-1 Flat sub-arc on A-36 plate with EM12K wire and F7A2 Flux.
13. WPS-SAW-2 Flat sub-arc on A-240(304L) plate with ER308L wire and Lincoln ST 100 Flux.
14. WPS-SAW-3 Flat sub-arc on A-240(316L) plate with ER316L wire and Lincoln ST 100 Flux.
15. WPS-SMAW-1 All position stick on A36 plate with E7018 3/32,1/8,5/32.
16. WPS-SMAW-2 Flat and horizontal stick on A36 plate with E7018 3/16,7/32,1/4 size wire.
17. WPS-SMAW-3 All position stick on A240(304L) plate with E308L-15 3/32,1/8,5/32.
18. WPS-SMAW-5 All position stick on A240(316L) plate with E316L-15 3/32,1/8,5/32.
19. WPS-SMAW-7 All position stick on A240(347) plate with E347-16 3/32,1/8,5/32.
20. WPS-SPR-1 Flat and horizontal spray arc on A36 plate with E70S-6 .045,and 1/16 size wire.
21. WPS-SPR-2 Flat and horizontal spray arc on A240(316L) plate with ER316L .045,and 1/16 size wire.
22. WPS-SPR-3 Flat and horizontal spray arc on A240(304L) plate with ER308L .045,and 1/16 size wire.
23. WPS-WRP-1 NOT PREQUALIFIED--But having this procedure will insure success with the most demanding X-ray and UT (Ultra-sonic) repairs. It will also help reduce the time required to develop your own PQR (Procedure Qualification Record).